As welded | ||
屈服強(qiáng)度 | 延伸率 | 抗拉強(qiáng)度 |
390 MPa | 45 % | 600 MPa |
As welded | |
沖擊值 | 測試溫度 |
135 J | 20 °C |
55 J | -196 °C |
Mn | Mo | Cu | C | Si | FN WRC-92 | Ni | N | Cr |
1.4 % | 3.6 % | 0.05 % | 0.01 % | 0.4 % | 7 % | 13.6 % | 18.9 % |
分類: | W18 15 3 L, EN ISO 14343-A, Wire Electrode, ER317L, SFA/AWS A5.9, Wire Electrode |
合金類型: | Austenitic (with approx. 8 % ferrite) 19% Cr - 12% Ni - 3% Mo - Low C |